J. Electron. Packag. June 2020, 142(2): 021004.
Paper No: EP-18-1042
Published Online: February 4, 2020
... and elevated temperature. The hardness, elastic modulus, and plasticity of Cu 6 Sn 5 and Cu 3 Sn at 25–200 °C are investigated by the nanoindentation method. The results show that the hardnesses of Cu 6 Sn 5 and Cu 3 Sn obey linear attenuation law with elevated temperature. The hardness of Cu 6 Sn 5 is more...